BJY 98 × 35.58 mm Neck Ring



A Wearing Part That Sets Mold Life
The neck ring holds the thread, the sealing lip and the support ring while the bottle is formed. It also absorbs the full clamping force of the machine on every cycle. When that insert reaches the end of its working life, the whole mold loses its ability to hold a clean neck, even though every other component remains serviceable.
What Abrasion Does to the Split Line
Repeated closing loads round off the split edges and dull the thread contour. Abrasive particles from regrind, together with water carryover, accelerate the process. The first symptom is usually a light burr under the thread. Later the thread itself loses definition, and capping heads begin to miss their torque targets, which shows up as slow leakage on stored pallets.
Hardening to HRC 53, Then Coating with DLC
BJY hardens the neck ring body to HRC 53, a level that keeps the split edges stable under continuous impact loading. The forming face then receives a DLC diamond coating. This layer offers high surface hardness and a very low friction coefficient, so polymer releases cleanly and does not stick at the cavity corners. The combined effect, proven across production campaigns, extends overall mold working life by more than 10%.
Replacement Inserts for Molds Already in Service
Worn neck rings are usually replaced rather than repaired. BJY machines individual replacements to the same reference as the original insert and checks the dimensions on a coordinate measuring table. Such inserts are ordered when an existing ring produces preform flash, distorts the thread or scores the sealing face. Installation needs no hand fitting, because the new ring seats in the pocket left by the old one. The line returns to clean production within one shift.